23 September 1998 Deformation of fused silica: nanoindentation and densification
Aril B. Shorey, Kai Xin, Kang-Hua Chen, John C. Lambropoulos
Author Affiliations +
Abstract
As compared to multicomponent optical glasses, when fused silica optical glass (pure SiO2) is ground or polished, it exhibits unique features, such as low surface microroughness and subsurface damage, low grinding-induced residual stresses, and low removal rates. On the other hand, fused silica glass is known to densify permanently when subjected to sufficiently large compressive stresses. Such densification, manifested as a permanent increase in the index of refraction, is facilitated by shear stresses. We discuss a simple constitutive model describing the densification of fused silica, under large applied model to interpret nanoidentification tests of fused silica over loads in the range 1 - 100 mN (about 0.1 - 10 gf) via finite element simulations of indentation of an axisymmetric half- space by a conical indenter with a spherical tip. Such geometry resembles the action of polishing and microgrinding abrasives used in optics manufacturing. The fused silica nanoindentation data are compared to other optical glasses such as BK7 and LHG8.
© (1998) COPYRIGHT Society of Photo-Optical Instrumentation Engineers (SPIE). Downloading of the abstract is permitted for personal use only.
Aril B. Shorey, Kai Xin, Kang-Hua Chen, and John C. Lambropoulos "Deformation of fused silica: nanoindentation and densification", Proc. SPIE 3424, Inorganic Optical Materials, (23 September 1998); https://doi.org/10.1117/12.323765
Lens.org Logo
CITATIONS
Cited by 15 scholarly publications.
Advertisement
Advertisement
RIGHTS & PERMISSIONS
Get copyright permission  Get copyright permission on Copyright Marketplace
KEYWORDS
Silica

Glasses

Abrasives

Polishing

Surface finishing

Optics manufacturing

Spherical lenses

RELATED CONTENT

Controlling stress in sapphire optics
Proceedings of SPIE (November 01 1997)
Finish machining of optical components in mass production
Proceedings of SPIE (March 01 1991)
Research of optical flats in pad polishing
Proceedings of SPIE (May 20 2009)
Inverse topographic analysis of scratches
Proceedings of SPIE (December 22 2003)

Back to Top