As the design rule shrinks, intra-field CD control becomes more difficult. Flare induced by lens contamination is one of CD variation sources across the exposed field and its distributions are different from tool to tool. To use the exposure tool with the contaminated lens, CD correction method is to be specified to improve the wafer CD uniformity. In this paper, the local flare values are measured using dose-to-clear method and CD measurement method in order to confirm the exposure tool condition. Then we design a mask whose transmittance is controlled locally for CD uniformity enhancement. The mask has several phase-out holes in the quartz side. By distributing the holes with respect to the local area flare, we can make the intensity distribution opposite to the lens local flare.
© (2003) COPYRIGHT Society of Photo-Optical Instrumentation Engineers (SPIE). Downloading of the abstract is permitted for personal use only.
Dong-Seok Nam, Gi-Sung Yeo, Jong Rak Park, Sung-Woon Choi, Sang-Gyun Woo, Han-Ku Cho, and Woo-Sung Han "Flare-induced CD variation correction using transmittance controlled mask", Proc. SPIE 5040, Optical Microlithography XVI, (26 June 2003); https://doi.org/10.1117/12.485409
Advertisement
Advertisement
RIGHTS & PERMISSIONS
Get copyright permission  Get copyright permission on Copyright Marketplace
KEYWORDS
Critical dimension metrology

Photomasks

Semiconducting wafers

Transmittance

Contamination

Cadmium

Control systems

RELATED CONTENT

New approach for 5X reticle CD methodology
Proceedings of SPIE (March 26 1993)
Goal-Oriented Process Tuning
Proceedings of SPIE (September 05 1980)
The study to enhance the mask global CD uniformity by...
Proceedings of SPIE (April 05 2007)
The study of contact hole MEEF and defect printability
Proceedings of SPIE (May 28 2004)

Back to Top