In this paper, we prepared carbon doped nanocrystalline ZnO by pyrolyzed zinc stearate at 250°C and 300°C respectively. The XRD curves indicate the sample has polycrystalline hexagonal wurtzite structure. The XRD data of the sample prepared at 250°C and 300°C has a bigger angle shift about 0.05°and 0.3°respectively. That indicate the structure of the sample has some changes. The EDS indicate the sample contains Zn, O and C. So the XRD shift may attribute to the C. The XPS indicate the C doped in the crystal lattice of ZnO of the sample prepared at 300°C, and the sample prepared at 250°C may be only a few of C doped in the crystal lattice of ZnO. The PL of the sample prepared at 300°C only has a weak ultraviolet emission, which indicates C modified the nanocrystalline ZnO surface as a non-radiative recombination center. In this process C could non-radiatively recombine the carries on the nanocrystallin ZnO surface. The sample prepared at 250°C has a strong visible emission at about 530 nm. This emission band could be attributed to oxygen vacancy because C schlepped some oxygen on the nanocrystalline ZnO surface.
Access to the requested content is limited to institutions that have purchased or subscribe to SPIE eBooks.
You are receiving this notice because your organization may not have SPIE eBooks access.*
*Shibboleth/Open Athens users─please
sign in
to access your institution's subscriptions.
To obtain this item, you may purchase the complete book in print or electronic format on
SPIE.org.
INSTITUTIONAL Select your institution to access the SPIE Digital Library.
PERSONAL Sign in with your SPIE account to access your personal subscriptions or to use specific features such as save to my library, sign up for alerts, save searches, etc.